Skip to content
Plate SIRIUS™ 4828
Plates

Plate SIRIUS™ 4828

Heat-resistant steel for furnaces and combustion chambers

Key parameters of Plate SIRIUS™ 4828
Grade 4828 / 1.4828 · UNS S30900
Standard EN 10095 / ASTM A240
Thickness 5–150 mm
Width 1250–3000 mm
Supplier INDUSTEEL (ArcelorMittal)
Lead time 8–12 weeks
ISO 9001:2015 EN 10204 3.1

Technical data

Technical data

Chemical composition [%]

Chemical composition of Plate SIRIUS™ 4828 in percent
C ≤ 0.20
Cr 19.0–21.0
Ni 11.0–13.0
Si 1.5–2.5

Mechanical properties

Mechanical properties Plate SIRIUS™ 4828
Yield strength Rp0.2 ≥ 230 MPa
Tensile strength Rm 550–800 MPa
Elongation A5 ≥ 30 %
Service temperature up to 1035 °C

Standard 309-type heat-resistant grade with higher silicon for better oxidation resistance.

Request a quote: Plate SIRIUS™ 4828

Upload drawing / PDF

Drag a file here or click to select

Sales department

Usually within 24 hours, depending on the complexity of the specification

+420 224 234 322 pragointer@pragointer.cz