Key parameters of Bar 22CrMoS3-5
Grade 22CrMoS3-5
Standard EN 10084
Diameter Ø 20–300 mm
Length 3000–12000 mm
Supplier Asil Çelik
Lead time 4–8 weeks
EN 10204 3.1

Technical data

Technical data

Chemical composition [%]

Chemical composition of Bar 22CrMoS3-5 in percent
C 0.19–0.25
Cr 0.65–0.95
Mo 0.45–0.60
S 0.020–0.040 (free-machining)

Mechanical properties

Mechanical properties Bar 22CrMoS3-5
Yield strength Rp0.2 after case hardening, depending on core
Tensile strength Rm ≈ 800–1100 MPa (core)
Surface hardness HRC 58–62 (after case hardening)

Sulphurised variant for better machinability: gears and shafts with a case-hardened surface.

Request a quote: Bar 22CrMoS3-5

Upload drawing / PDF

Drag a file here or click to select

Sales department

Usually within 24 hours, depending on the complexity of the specification

+420 224 234 322 pragointer@pragointer.cz