Skip to content
Ship Plate E
Marine materials

Ship Plate E

Ship plate with guaranteed impact toughness at −40 °C

Key parameters of Ship Plate E
Grade Grade E
Standard classification rules (IACS)
Thickness 5–50 mm
Width 1500–4000 mm
Supplier Baglietto S.r.l.
Lead time 1 week (in stock)
Lloyd's Register BV, DNV, RINA, ABS

Technical data

Technical data

Chemical composition [%]

Chemical composition of Ship Plate E in percent
C ≤ 0.18
Mn 0.70–1.60
Si ≤ 0.35

Mechanical properties

Mechanical properties Ship Plate E
Yield strength ReH ≥ 235 MPa
Tensile strength Rm 400–520 MPa
Impact toughness at −40 °C ≥ 27 J

The highest toughness class within normal strength: structures for polar and northern waters.